Welcome Jiangsu Haohua Industry Group Website Map
Location : home > Materials > Nickel Alloys >

Nickel Alloy 600


Physical Properties of Nickel Alloy 600 in the Annealed Condition at -20°F to +100°F

 

      Tensile Strength Yield Strength            
Alloy UNS Designation Spec. psi MPa ksi psi MPa ksi Elongation in 2 in. (min.) % Grain Size Req. Max. Hardness Modulus of Elasticity (x106psi) Mean Coefficient of Thermal Expansion (IN./IN./°F x 10-6) Thermal Conductivity (BTU-in/ ft2-h-°F)
600 N06600 B516, B517 80,000 550 80 35,000 240 35 30 — — 30 6.9 103

 

Composition of Nickel Alloy 600 tubing and pipe

 

Grade 600
UNS Designation N06600
Nickel (Ni) 72.0 Min. plus Cobalt
Chromium (Cr) 14.00–17.00
Iron (Fe) 6.0–10.0
Molybdenum (Mo) —
Titanium (Ti) Max. —
Aluminum (Al) Max. —
Cobalt (Co) Max. —
Tungsten (W) —
Vanadium (V) Max. —
Copper (Cu) Max. 0.5
Manganese (Mn) Max. 1.0
Niobium (Nb) plus Tantalum —
Carbon (C) Max. 0.15
Nitrogen (N) Max. —
Silicon (Si) Max. 0.5
Sulphur (S) Max. 0.015
Phosphorous (P) Max. —
Other Elements —

 

Nickel Alloy 600 Product Range

 

Alloy UNS Designation Werkstoff NR. Specifications*
600 N06600 2.4816 B/SB516, B/SB517

 

*Note: The specifications noted including ASTM, ASME, or other applicable authorities are correct at the time of publication. Other specifications may apply for use of these materials in different applications.