Super Austenitic N08811 Alloy


Physical Properties of Super Austenitic N08811 Alloy in the Annealed Condition at -20°F to +100°F

      Tensile Strength Yield Strength            
Alloy UNS Designation Spec. psi MPa ksi psi MPa ksi Elongation in 2 in. (min.) % Grain Size Req. Max. Hardness Modulus of Elasticity (x106psi) Mean Coefficient of Thermal Expansion (IN./IN./°F x 10-6) Thermal Conductivity (BTU-in/ ft2-h-°F)
800HT N08811 B514, B515 65,000 450 65 25,000 170 25 30 5 & coarser — — 7.9 80

 

Composition of Super Austenitic N08811 tubing and pipe

Grade N08811
UNS Designation N08811
Nickel (Ni) 30.0– 35.0
Chromium (Cr) 19.0–23.0
Iron (Fe) 39.5 Min.
Molybdenum (Mo) —
Titanium (Ti) Max. 0.15–0.60*
Aluminum (Al) Max. 0.15–0.60
Cobalt (Co) Max. —
Tungsten (W) —
Vanadium (V) Max. —
Copper (Cu) Max. 0.75
Manganese (Mn) Max. 1.5
Niobium (Nb) plus Tantalum —
Carbon (C) Max. 0.06–0.10
Nitrogen (N) Max. —
Silicon (Si) Max. 100
Sulphur (S) Max. 0.1015
Phosphorous (P) Max. —
Other Elements —

 

Super Austenitic N08811 Product Range

UNS Designation Werkstoff NR. Specifications*
N08811 1.4876 B/SB515, B/SB514

*Note: The specifications noted including ASTM, ASME, or other applicable authorities are correct at the time of publication. Other specifications may apply for use of these materials in different applications.