Ferritics Alloys S44627


Physical Properties of S44627 Alloys in the Annealed Condition at -20°F to +100°F

    Tensile Strength Yield Strength            
UNS Designation Spec. psi MPa ksi psi MPa ksi Elongation in 2 in. (min.) % Grain Size Req. Max. Hardness Modulus of Elasticity (x106psi) Mean Coefficient of Thermal Expansion (IN./IN./°F x 10-6) Thermal Conductivity (BTU-in/ ft2-h-°F)
S44627 A268 65,000 450 65 40,000 275 65 12* — 95 Rb 29.0 5.2 116

*for 0.049” average wall

Composition of S44627 tubing and pipe

UNS Designation S44627
Nickel (Ni) 0.5*
Chromium (Cr) 25.0–27.5
Iron (Fe) Bal.
Molybdenum (Mo) 0.75–1.50
Titanium (Ti) Max. —
Aluminum (Al) Max. —
Cobalt (Co) Max. —
Tungsten (W) —
Vanadium (V) Max. —
Copper (Cu) Max. 0.2
Manganese (Mn) Max. 0.40
Niobium (Nb) plus Tantalum 0.05–0.20
Carbon (C) Max. 0.01* **
Nitrogen (N) Max. 0.015
Silicon (Si) Max. 0.40
Sulphur (S) Max. 0.02
Phosphorous (P) Max. 0.02
Other Elements —

*Nickel + Copper

**0.015 Max. for OD<0.500" and for T<0.049"

S44627 Product Range

UNS Designation Werkstoff NR. Specifications*
S44627 N/A A267/SA267

*Note: The specifications noted including ASTM, ASME, or other applicable authorities are correct at the time of publication. Other specifications may apply for use of these materials in different applications.